<< Back
| Topic: Paint 3 stage process | | Question | | Can you paint signfoam3 in a 3 stage process, much like an automobile; laquer primer, enamel paint, auto urathane clear? Is there any problem with expanding or contracting of Sign•Foam3, the urathane dries very hard, would there be any problems with the urathane cracking? | | Answer | The painting process you describe has been done quite successfully with Sign•Foam. As long as you are using at least 15 lb. material the expansion will not be an issue.
Thanks
Tech Support
| Tech Support |
| | |
|
|